Chinese Journal of Tissue Engineering Research ›› 2015, Vol. 19 ›› Issue (21): 3392-3397.doi: 10.3969/j.issn.2095-4344.2015.21.021
Previous Articles Next Articles
Nie Er-min, Jiang Rui, Zhang Chun-yuan, Zeng Jin-di, Tan Ji-zhou
Online:
2015-05-21
Published:
2015-05-21
Contact:
Zhang Chun-yuan, Professor, Department of Stomatology, the First Affiliated Hospital of Sun Yat-sen University, Guangzhou 510080, Guangdong Province, China
About author:
Nie Er-min, Master, Attending physician, Department of Stomatology, the First Affiliated Hospital of Sun Yat-sen University, Guangzhou 510080, Guangdong Province, China
Supported by:
the Social Development Project of Guangdong Provincial Science and Technology Department, No. 2011B080701010, 2011B080701086, 2012B061700066
CLC Number:
Nie Er-min, Jiang Rui, Zhang Chun-yuan, Zeng Jin-di, Tan Ji-zhou. Clinical application of temporary crown and cement materials: physical properties and biological safety[J]. Chinese Journal of Tissue Engineering Research, 2015, 19(21): 3392-3397.
[1] Carle D,Shope B,Ogrodnick D.Temporary crowns.J Vet Dent. 2013;30(1):34-38.
[2] Roe P,Patel RD.Fabrication of a modified repositioning key for relining provisional restorations.J Prosthet Dent.2010;104(6): 401-402.
[3] Balkenhol M,Ferger P,Mautner MC,et al.Provisional crown and fixed partial denture materials:Mechanical properties and degree of conversion.Dent Mater,2007;23(12):1574-1583.
[4] Burke FJ,Murray MC,Shortall AC.Trends in indirectdentistry: 6. Provisional restorations, more than just atemporary. Dent Update.2005;32(8):443-444,447-448, 450-452.
[5] Strassler HE.Fixed prosthodontics provisional materials: making the right selection. Compend Contin Educ Dent. 2013; 34(1):22-24,26.
[6] Tüzüner T,Ku?göz A,Nur BG.Temporary management of permanent centralincisors loss caused by trauma in primarydentition with natural crowns: a case report.Dent Traumatol.2009;25(5):522-526.
[7] Hammond BD,Cooper JR 3rd,Lazarchik DA.Predictable repair of provisional restorations.J EsthetRestor Dent.2009; 21(1):19-24.
[8] Balkenhol M,Mautner MC,Ferger P,et al.Mechanical properties of provisional crown and bridgematerials: chemical-curing versus dual-curing systems.J Dent.2008; 36(1):15-20.
[9] Balkenhol M,Knapp M,Ferger P,et al.Correlation between polymerization shrinkage andmarginal fit of temporary crowns. Dental Mater.2008;24(11):1575-1584.
[10] Kim SH,Watts DC.Polymerization shrinkage-strain kineticsof temporary crown and bridge materials. Dent Mater.2004;20(1): 88-95.
[11] Kim SH,Watts DC.Effect of glass-fiber reinforcement andwater storage on fracture toughness of polymer- basedprovisional crown and FPD materials.Int J Prosthodont. 2004;17(3):318-322.
[12] Kim SH,Watts DC.In vitro study of edge-strength of provisional polymer-basedcrown and fixed partial denture materials.Dent Mater.2007;23(12):1570-1573.
[13] Vally Z,Sykes LM,Aspeling ME,et al.In vitro comparison of the compressive strengths of seven different provisional crown materials.SADJ.2013;68(2):64-67.
[14] Poonacha V,Poonacha S,Salagundi B,et al.In vitro comparison of flexural strength and elastic modulus of three provisional crown materials used in fixed prosthodontics. J Clin Exp Dent.2013;5(5):e212-217.
[15] Al Twal EQ,Chadwick RG.Fibre reinforcement of two temporary composite bridge materials--effect upon flexural properties.J Dent.2012;40(12):1044-1051.
[16] Garoushi SK,Vallittu PK,Lassila LV. Short glass fiber-reinforced composite with a semi-interpenetrating polymer network matrix for temporary crowns and bridges. J Contemp Dent Pract.2008;9(1):14-21.
[17] Nejatidanesh F,Lotfi HR,Savabi O.Marginal accuracy ofinterim restorations fabricated from four interimautopolymerizing resins. J Prosthet Dent. 2006;95(5):364-367.
[18] Hansen PA,Sigler E,Husemann RH.Making multiple predictable single-unit provisional restorations using an indirect technique.J Prosthet Dent. 2009;102(4):260-263.
[19] Hamza TA,Rosenstiel SF,Elhosary MM,et al.Theeffect of fiber reinforcement on the fracture toughness andflexural strength of provisional restorative resins. J Prosthet Dent.2004; 91(3): 258-264.
[20] Ha SR,Yang JH,Lee JB,et al.Comparison of polymer-based temporary crown and fixed partial denture materials by diametral tensile strength.J Adv Prosthodont. 2010;2(1): 14-17.
[21] Akova T,Ozkomur A,Uysal H.Effect of food-simulatingliquids on the mechanical properties of provisionalrestorative materials. Dent Mater.2006;22(12):1130-1134.
[22] Hamza TA,Rosenstiel SF,El-Hosary MM,et al.Fracture resistance of fiber-reinforced PMMA interim fixedpartial dentures. J Prosthodont. 2006;15(4):223-228.
[23] Balkenhol M,Köhler H,Orbach K,et al.Fracture toughness of cross-linked and non-cross-linkedtemporary crown and fixed partial denture materials.Dent Mater. 2009;25(7):917-928.
[24] Debnath S,Ranade R,Wunder SL,et al.Interface effects on mechanical properties ofparticle-reinforced composites.Dent Mater.2004;20(7):677-686.
[25] Gujjari AK,Bhatnagar VM,Basavaraju RM.Color stability and flexural strength of poly (methyl methacrylate) and bis-acrylic composite based provisional crown and bridge auto-polymerizing resins exposed to beverages and food dye: an in vitro study. Indian J Dent Res.2013;24(2):172-177.
[26] Givens EJ Jr,Neiva G,Yaman P,et al.Marginal Adaptation and Color Stability of Four ProvisionalMaterials.J Prosthodont. 2008;17(2):97-101.
[27] Watts DC.Reaction kinetics and mechanics inphoto-polymerised networks.Dent Mater,2005;21(1):27-35.
[28] Stansbury JW,Trujillo-Lemon M,Lu H,et al. Conversion-dependent shrinkage stress and strain in dentalresins and composites.Dent Mater.2005;21(1):56-67.
[29] Dewaele M,TruffierBoutry D,Devaux J,et al. Volumecontraction in photocured dental resins: theshrinkage-conversion relationship revisited.Dent Mater. 2006;22(4):359-365.
[30] Ellakwa A,Cho N,Lee IB.The effect of resin matrixcomposition on the polymerization shrinkage andrheological properties of experimental dental composites.Dent Mater.2007;23(10): 1229-1235.
[31] Atai M,Watts DC.A new kinetic model for thephotopolymerization shrinkage-strain of dental compositesand resin-monomers.Dent Mater.2006;22(8):785-791.
[32] Baroudi K,Saleh AM,Silikas N,et al.Shrinkagebehaviour of flowable resin-composites related toconversion and filler-fraction. J Dent. 2007;35(8):651-655.
[33] Ehrenberg D,Weiner GI,Weiner S.Long-term effects ofstorage and thermal cycling on the marginal adaptation ofprovisional resin crowns: a pilot study. J Prosthet Dent.2006;95(3): 230-236.
[34] Yu YQ,Zou DR,Su JS.The study of the monomer release from four kinds of temporary crown material by infrared spectrum. Shanghai Kou Qiang Yi Xue.2008;17(6):643-647.
[35] Ramkumar V,Sangeetha A,Kumar V.Effect of water temperature on the fit of provisional crown margins during polymerization: An in vitro study. J Pharm Bioallied Sci.2012; 4(Suppl2):S376-383.
[36] Cardoso M,Torres MF,Rego MR,et al.Influence of application site of provisional cement on the marginal adaptation of provisional crowns.J Appl Oral Sci.2008;16(3):214-218.
[37] Akova T,Ozkomur A,Dundar C,et al.Intrapulpal heat generation during provisionalization: effect of desensitizer and matrix type. J Prosthodont. 2008;17(2):108-113.
[38] Altintas SH,Yondem I,Tak O,et al.Temperaturerise during polymerization of three different provisionalmaterials.Clin Oral Investig.2008;12(3):283-286.
[39] Michalakis K,Pissiotis A,Hirayama H,et al.Comparison of temperature increase in the pulp chamberduring the polymerization of materials used for the directfabrication of provisional restorations.J Prosthet Dent.2006;96(6):418-423.
[40] Chiodera G,Gastaldi G,Millar BJ.Temperature change inpulp cavity in vitro during the polymerization of provisionalresins. Dental Mater.2009;25(3):321-325.
[41] Usumez A,Ozturk AN,Aykent F.The effect of dentindesensitizers on thermal changes in the pulp chamberduring fabrication of provisional restorations.J Oral Rehabil. 2004;31(6):579-584.
[42] Kim SH,Watts DC.Exotherm behavior of the polymer-basedprovisional crown and fixed partial denture materials.Dental Mater.2004;20(4):383-387.
[43] Bevilacqua L,Biasotto M,Cadenaro M,et al. Reaction exothermia of 2 relining resins for temporarycrowns. Minerva Stomatol.2005;54(1-2):35-41.
[44] Seelbach P,Finger WJ,Ferger P,et al.Temperature rise on dentin caused by temporary crown andfixed partial denture materials: Influencing factors.J Dent. 2010;38(12):964-973.
[45] Hattori N,Suzuki T,Jinno S,et al.Methyl methacrylate activates the Gsta1 Promoter.J Dent Res.2008;87(12):1117-1121.
[46] Perry RD,Magnuson B.Provisional materials: key components of interim fixed restorations. Compend Contin Educ Dent. 2012; 33(1):59-60,62.
[47] Polydorou O,Hammad M,König A,et al.Release of monomers from different core build-up materials、Dent Meter. 2009;25(9): 1090-1095.
[48] Lung CY,Darvell BW.Minimizationofthe inevitable residualmonomer in denturebaseacrylic.Dent Meter. 2005; 21(9):1119-1128.
[49] Bettencourt AF,Neves CB,de Almeida MS,et al. Biodegradation of acrylicbasedresins: Areview. Dent Meter,2010;26(5):171-180.
[50] Danesh G, LippoldC, MischkeKL, et al. Polymerization characteristics of light- and auto-curing resins for individual splints.Dent Mater.2006;22(4):426-433.
[51] VanLanduyt KL,Nawrot T,Geebelen B,et al. How muchdo resin- based dental materials release? A meta-analytical approach.Dent Meter.2011;27(7):723-747.
[52] Bural C,Aktas E,Deniz G,et al.Effect of post-polymerization heat-treatmentson degreeofconversion,leaching residual MMA and in vitro cytotoxicity of autopolymerizing acrylic repair resin. Dent Meter.2010;27(4):1135-1143.
[53] Ulker M,Ulker HE,Zortuk M,et alEffects of current provisionalrestorationmaterialsontheviabilityoffibroblasts. EurJ Dent.2009;3(2):114-119.
[54] Kleinsasser NH,Schmid K,Sassen AW,et al. Cytotoxic and genotoxic effects of resin monomers in human salivary gland tissue and lymphocytes as assessed by the single cell microgel electrophoresis (Comet) assay. Biomaterials. 2006; 27(9):1762-1770.
[55] Samuelsen JT,Dahl JE,Karlsson S. Apoptosis induced by themonomersHEMA and TEGDMA involves formation of ROS and differential activation of the MAP-kinases p38, JNK and ERK. Dent Meter.2007;23(1):34-39.
[56] Haselton DR,Diaz-Arnold AM,Dawson DV.Effect of storage solution on surface roughness of provisional crown and fixed partial denture materials.J Prosthodont. 2004;13(4):227-232.
[57] Balkenhol M,Meyer M,Michel K,et al. Effect of surface condition and storage time on therepairability of temporary crown and fixed partial denturematerials.J Dent. 2008;36(11):861-872.
[58] Ayuso-Montero R,Martinez-Gomis J,Lujan-Climent M,et al.Influence of matrix type on surface roughness of three resins for provisional crowns and fixed partial dentures.J Prosthodont.2009;18(2):141-144.
[59] Orug BO,Baysallar M,Centiner D,et al.Increased antibacterial activity of zinc polycarboxylate cement by the addition of chlorhexidinegluconate in fixed prosthodontics.Int J Prosthodont.2005;18(5):377-382.
[60] Lewinstein I,Chweidan H,Matalon S,et al.Retention and marginal leakage of provisional crowns cemented with provisional cements enriched with chlorhexidinediacetate.J Prosthet Dent.2007;98(5):373-378.
[61] Chiramana S,Siddineni KC,Jyothula RR,et al.Evaluation of the Luting Cement Spacefor Provisional Restoration by using Various Coats of Die Spacer Materials-An Invitro Study.J Clin Diagn Res.2014;8(9):ZC22-25.
[62] Rego MR,Santiago LC.Retention of provisional crowns cemented with eight temporary cements: comparative study.J Appl Oral Sci.2004;12(3):209-212.
[63] Kanakuri Kl,Kawamoto Y,Kakehashi Y,et al.Influence of temporary cements on bond strength between resin-based luting agents and dentin.Am J Dent.2006;19(2):101-105.
[64] Dersley G, Masri R.A technique to recement provisional crowns by reactivating residualzinc oxide-eugenol cement.J Prosthet Dent.2006;95(5):397-398.
[65] Mosharraf R.A simple method for cleaning zinc oxide-eugenol provisionalcement residues from the intaglio surface of casting restorations.J Prosthet Dent. 2004;91(2):200.
[66] Kanakuri K,Kawamoto Y,Matsumura H.Influence of temporary cement remnant and surface cleaning method on bond strength to dentin of a composite luting system. J Oral Sci. 2005; 47(1):9-13. |
[1] | Pu Rui, Chen Ziyang, Yuan Lingyan. Characteristics and effects of exosomes from different cell sources in cardioprotection [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(在线): 1-. |
[2] | Zhang Chao, Lü Xin. Heterotopic ossification after acetabular fracture fixation: risk factors, prevention and treatment progress [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(9): 1434-1439. |
[3] | Zhou Jihui, Li Xinzhi, Zhou You, Huang Wei, Chen Wenyao. Multiple problems in the selection of implants for patellar fracture [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(9): 1440-1445. |
[4] | Wang Debin, Bi Zhenggang. Related problems in anatomy mechanics, injury characteristics, fixed repair and three-dimensional technology application for olecranon fracture-dislocations [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(9): 1446-1451. |
[5] | Ji Zhixiang, Lan Changgong. Polymorphism of urate transporter in gout and its correlation with gout treatment [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(8): 1290-1298. |
[6] | Yuan Mei, Zhang Xinxin, Guo Yisha, Bi Xia. Diagnostic potential of circulating microRNA in vascular cognitive impairment [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(8): 1299-1304. |
[7] | Wang Xianyao, Guan Yalin, Liu Zhongshan. Strategies for improving the therapeutic efficacy of mesenchymal stem cells in the treatment of nonhealing wounds [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1081-1087. |
[8] | Wan Ran, Shi Xu, Liu Jingsong, Wang Yansong. Research progress in the treatment of spinal cord injury with mesenchymal stem cell secretome [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1088-1095. |
[9] | Liao Chengcheng, An Jiaxing, Tan Zhangxue, Wang Qian, Liu Jianguo. Therapeutic target and application prospects of oral squamous cell carcinoma stem cells [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1096-1103. |
[10] | Zhao Min, Feng Liuxiang, Chen Yao, Gu Xia, Wang Pingyi, Li Yimei, Li Wenhua. Exosomes as a disease marker under hypoxic conditions [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1104-1108. |
[11] | Xie Wenjia, Xia Tianjiao, Zhou Qingyun, Liu Yujia, Gu Xiaoping. Role of microglia-mediated neuronal injury in neurodegenerative diseases [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1109-1115. |
[12] | Li Shanshan, Guo Xiaoxiao, You Ran, Yang Xiufen, Zhao Lu, Chen Xi, Wang Yanling. Photoreceptor cell replacement therapy for retinal degeneration diseases [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1116-1121. |
[13] | Jiao Hui, Zhang Yining, Song Yuqing, Lin Yu, Wang Xiuli. Advances in research and application of breast cancer organoids [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1122-1128. |
[14] | Wang Shiqi, Zhang Jinsheng. Effects of Chinese medicine on proliferation, differentiation and aging of bone marrow mesenchymal stem cells regulating ischemia-hypoxia microenvironment [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1129-1134. |
[15] | Zeng Yanhua, Hao Yanlei. In vitro culture and purification of Schwann cells: a systematic review [J]. Chinese Journal of Tissue Engineering Research, 2021, 25(7): 1135-1141. |
Viewed | ||||||
Full text |
|
|||||
Abstract |
|
|||||