Chinese Journal of Tissue Engineering Research ›› 2011, Vol. 15 ›› Issue (25): 4655-4657.doi: 10.3969/j.issn.1673-8225.2011.25.023

Previous Articles     Next Articles

Effect of Panavia F resin adhesive on tetracycline stained teeth mask with different simulated staining levels following Cerinate porcelain veneer repair

Shang Wei-rong1, Gao Shi-jun2, Yuan Wen-jun2   

  1. 1Community Health Center, Social Business Development Council of Changchun High-tech Development Zone, Changchun  130012, Jilin Province, China
    2Department of Prosthodontics, Second Affiliated Hospital (Stomatological Hospital) of Jiamusi University, Jiamusi  154002, Heilongjiang Province, China
  • Received:2011-03-16 Revised:2011-05-16 Online:2011-06-18 Published:2014-01-10
  • About author:Shang Wei-rong★, Master, Master’s supervisor, Professor, Community Health Center, Social Business Development Council of Changchun High-tech Development Zone, Changchun 130012, Jilin Province, China koujieswr@163.com

Abstract:

BACKGROUND: Aesthetic repair on tetracycline stained teeth is mostly confined to the clinical observation, while the experimental study is relatively few.
OBJECTIVE: To study the color changes of Cerinate porcelain veneer repaired tetracycline stained teeth: mild (yellow), moderate (dark gray), severe (yellow-gray), very severe (taupe).
METHODS: Simulated tetracycline stained teeth were divided according to staining degree into four groups: mild, moderate, severe, and very severe groups; each group had ten specimens which were repaired with Cerinate porcelain veneer, bonded with Panavia F opaque resin adhesive. The L*, a*, b* values of specimens before and after bonding was measured by electronic color measurement instrument.
RESULTS AND CONCLUSION: Before and after bonding, the values of L*, a*, b* were significantly different (P < 0.05). Mild tetracycline stained teeth bonded using resin adhesive without opaque bonding have a better effect than moderate and severe tetracycline stained teeth bonded with opaque resin adhesive; while, it is best to use other restorations to repair very severe tetracycline stained teeth.